Specifications Data
Material Polypropylene
Serialization Barcode and human-readable equivalent is digitally printed – providing excellent clarity and easy scanning. Code 39 is the standard symbology with a range of 2.7 to 9.4 CPI (characters per inch). Optional linear and 2D symbologies available. Although this product is primarily marketed as a bar code product, we can produce it with human-readable numbers only or unserialized.
Label Copy The label copy may include block type, stylized type, logos or other designs
Colors Standard colors include black, red, yellow, green or blue. Custom spot colors are also available at no additional charge. Due to contrast needed for the bar code scanner, all bar codes are black.
Standard Adhesive High performance adhesive
Frequency Range 860-960 MHz
Sizes 4" x 1.25"
Packaging Produced and shipped in roll form.
Shipment 14 business days

Price Table

Size 1 - 299 300 - 499 500 - 999 1000 - 2999 3000 - 4999 5000 - 6999 7000 - 9999
3.95" x 1.18" $2.08 $1.15 $0.78 $0.50 $0.41 $0.32 $0.29

Color Price Table

Size 1 - 299 300 - 499 500 - 999 1000 - 2999 3000 - 4999 5000 - 6999 7000 - 9999
3.95" x 1.18" $2.24 $1.26 $0.88 $0.55 $0.44 $0.35 $0.32

Race bibs

Chemical Test Summary
All inlays still reading after 48 hours of exposure - even when wet.
Chemical Test Data
Water Salt Water Bathroom Cleaner Glass Cleaner Isopropanol Brake Fluid Acetone Diesel Fuel Nitric Acid Hydrochloric Acid Sodium Hydroxide
2 hours NE loss of adhesion to glass panel loss of adhesion to glass panel loss of adhesion to glass panel Tag delaminated No effect Loss of adhesion to glass panel,tag delaminated adhesive ooze loss of adhesion to glass panel loss of adhesion to glass panel loss of adhesion to glass panel
24 hours No effect loss of adhesion to glass panel loss of adhesion to glass panel loss of adhesion to glass panel,tag delaminated Tag delaminated No effect loss of adhesion to glass panel,tag delaminated Adhesive ooze loss of adhesion to glass panel loss of adhesion to glass panel loss of adhesion to glass panel
48 hours Tag delaminated loss of adhesion to glass panel,Tag delaminated loss of adhesion to glass panel,Tag delaminated loss of adhesion to glass panel,Tag delaminated loss of adhesion to glass panel,Tag delaminated loss of adhesion to glass panel loss of adhesion to glass panel,Tag delaminated Adhesive ooze,Tag delaminated loss of adhesion to glass panel loss of adhesion to glass panel loss of adhesion to glass panel
Temperature Test Summary
Samples exposed to each temperature for 1 hour. *Sample started to melt, but inlay was still reading and read after exposure to 350F. After exposure to 400F, inlay would not read.
Temperature Test Data
150F 200F 250F 300F 350F 400F
No effect Sample shrinking, adhesive ooze at edges Sample shrinking, adhesive ooze at edges Tag melted/destroyed* Tag melted/destroyed Tag melted/destroyed
Read Range Test Summary
Real world testing showed a read range of 28 feet with a Motorola MC9090 handheld reader set to 30 dbm.